1. Put your piece in a room temperature kiln, and set the kiln temperature at 500 Deg.C (932F)
2. Ramp up until 500 Deg. C (932F) and hold for 30 mins.
3. Set the kiln temp at 870 Deg. C (1598F), and hold it at 870 Deg.C for 60 mins.
4. Turn off the kiln and wait until the kiln temperature drops to 200 Deg.C (392F)
5. Take the piece out and wait until the piece cools down completely or leave it until the kiln temperature drops to room temperature.